Troubleshooting guide › Fix it yourself, by machine › ARC transformers and rectifiers

Fix it yourself: Cruxweld AC arc transformers (CWA-ARC series) and DC welding rectifiers (CWR-400D, CWR-600D)

Transformer machines and rectifiers are the workhorses that run for 20 years. They have no electronics to fail, so when one stops it is almost always a connection, a fuse, a phase or the fan. This page is for the CWA-ARC AC series (moving-core current control) and the CWR diode rectifiers (transductor control).

Covers: ARC 220 / 320 / 350 / 450 A transformer welders (CWA-ARC series), Welding Rectifier 400 / 600 (CWR-400D, CWR-600D), thyristor rectifiers.

Reviewed by the Cruxweld technical team, October 2026. Settings are starting points to confirm on a test piece; acceptance is decided by the code or drawing the job is built to. Checks marked “call” are for our technical team.

Before you start: Switch the machine off at its own switch and at the distribution box before touching any cable, torch or connection. Everything on this page is outside the cabinet: supply, cables, consumables, gas, air, water and settings. If a check below does not clear the fault, stop there and send us the symptom; opening the machine is for our technical team. Change range links, polarity cables or the STANDARD/REMOTE switch only with the machine off.

Five checks before you call

  1. Supply: both lines on a 2-phase transformer, all three phase lamps lit on a rectifier; mains fuse and isolator contacts.
  2. Output: holder and work cables tight at the terminals, clamp on bright metal, no broken strands at the lugs.
  3. Fan: runs when the main switch is on; louvres clear; 0.5 m free space around the machine.
  4. Controls: range links on the right range, STANDARD selected unless a remote is connected, polarity cables as the electrode needs (rectifiers).
  5. Electrodes: dry; current in the packet range.

Fault table: what you see, what to check, when to call

What you seeCheck yourselfIf it persists
Machine does not power up, lamps offSupply on both/all lines; mains fuse; isolator contacts; ON/OFF switch; control fuse (rectifier)Control transformer: call
One phase lamp off (rectifier)A phase is missing: stop weldingSupply or mains fuse; do not weld on two phases
Machine on, no output, fan runsCables and lugs; work clamp; output terminals tight; machine not overheated; REMOTE selected with no remoteCall
Fan does not run, output normalFan fuse (rectifier); fan turns freely by hand (isolated); fan leadsFan motor: call. Do not weld long without the fan
Welding current erraticLoose mains or welding connections; damp electrodes; supply fluctuating; worn regulator contactRegulator: call
Weak, sluggish arcCurrent too low or LOW range selected; low supply voltage; cables too long or thin; loose connectionCall with the supply reading
Current cannot be adjusted / handle stiff (transformer)Lead screw and shunt dry or dirty; anti-noise screws over-tightenedGrease the screw (high-temperature grease); shunt mechanism: call
Only minimum current, will not increase (rectifier)Control fuse; regulator knob; range linksControl transformer or rectifier: call
Control fuse blows repeatedly (rectifier)Nothing outsideControl transformer, fan or regulator: call
Excessive spatter, unstable arcCurrent too high; arc too long; damp electrodes; wrong polarity (rectifier)Failed diode on a rectifier: call
Machine overheatsDuty cycle; louvres blocked; dust inside; fan not runningLet it cool with the fan running; if it overheats at low current: call
Loud humming or rattling (transformer)Normal hum is fine; a rattle is the shunt or a loose panelA qualified person tightens the anti-noise screws a quarter turn at a time; tighten panels
Mains fuse blowsFuse rating as recommended (63 A for a 450 A transformer); input cable for damageShort circuit in the primary or diodes: call

Care schedule

  • Daily: cables, holder, clamp; louvres clear; all phase lamps lit; run unloaded 3 minutes after welding so the fan cools the transformer.
  • Every 3 months: cable insulation; clean and tighten output terminals and range links.
  • Every 6 months (isolated): blow dust out with dry low-pressure air, monthly in dusty shops; check fan mounting; tighten diode and transformer connections (rectifier).
  • Yearly: grease the moving shunt and lead screw (transformer); a qualified electrician checks input terminals, earth, insulation and diodes.

Questions we get asked

Why does the ammeter not match the current I expect?

The scale on a transformer machine is approximate; the actual current depends on supply voltage, cable length and arc length. Set by the bead and the electrode range, not by the pointer.

Rectifier or inverter for my shop?

A rectifier is simpler, tolerant of dust and rough supply, and has no boards to fail; an inverter is lighter, more efficient and has hot start and arc force. For a fixed bay with heavy electrodes, many shops still prefer the rectifier.

Welding or cutting problem rather than a machine fault?

If the machine runs but the weld or cut is wrong, the cause is usually settings, consumables or the material. Start here:

Does the machine matter?

A transformer machine that overheats is being run over its duty cycle: 60 % at the rated current, continuous at about 75 % of it. Overheating damages the transformer insulation and that is a workshop repair, so respect the rest periods or move up a size.

Still stuck?

Send a photo of the weld or cut, your machine model, consumable and plate thickness. Our technical team replies on WhatsApp with the likely causes and the next checks to make.

45+ years of welding expertise · GeM Registered OEM Manufacturer · Supported Worldwide

WhatsApp chat